1. TM—M007/–TXX
2. JL—M070/—–
3. JO-03M077/—–
1. Oak veneer sanded with 180 grit paper. Spray application of TM-M007 / Txx series basecoat. Drying for 1 hour.
2. Spray two coats of JL — M070 with an interval of 8 hours and sanded with 320 grit paper. After the second coat, dry for 12 hours and lightly sand with 320 grit paper.
3. Apply JO-03M077. Dry for 24 hours.